Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.97 MPa | 286 psi | ASTM D412 |
Polymax® Maxelast® P1745N TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 1.97 MPa | 286 psi | ASTM D412 |
Polymax® Maxelast® P2635 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 1.97 MPa @Strain 100 % |
286 psi @Strain 100 % |
|
Saint-Gobain Tygon® E-1000 Ultra-Soft Laboratory Tubing Soft and flexible, Tygon® E-1000 Non-DEHP laboratory tubing delivers the same performance in a formulation that contains non-DEHP [Bis (2-ethylhexyl) phthalate] plasticizers. The market demand a.. |