Polymer Property : Tensile Strength, Yield = 10.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.8 MPa
1570 psi
-10% change after 70 hours @ 100°C; ASTM D412
Precision Polymer Engineering N75L Nitrile Rubber
Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. Ultra-Low acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet ASTM D2000/SAE J200 line call-out: MBF710, B34, F19.Application..
Tensile Strength, Yield 10.8 MPa
1570 psi
ASTM D638
Chevron Phillips 1400 Injection Molding Resin  (discontinued **)
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 24200Characteristics: Good Flexibility, Good Flow, Good Warping Resistance, Good Mold Release, Good ESCRApplications:Lids & Closures, C..
Tensile Strength, Yield 10.8 MPa
1570 psi
500 mm/min; ASTM D638
Eastman 1840A Polyethylene  (discontinued **)
Polyethylene 1840A is a low-density formulation with no slip or antiblock. It is suggested for injection molding applications requiring good stiffness, gloss, good processability or layflat properti..
Tensile Strength, Yield 10.8 MPa
1570 psi
500 mm/min; ASTM D638
Eastman 1840E Polyethylene  (discontinued **)
Polyethylene 1840E is a low-density formulation for general extrusion.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer app..
Tensile Strength, Yield 10.8 MPa
1560 psi
ASTM D638
LyondellBasell Purell® PE1840H Low Density Polyethylene, Blown Film, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding
Purell PE 1840 H is a low density polyethylene with good flexibility and is delivered in pellet form. It is designed for small blow molding but can also be used in film applications and injection mo..
Tensile Strength, Yield 10.8 MPa
1560 psi
100%; ASTM D412
Teknor Apex APEX® 3300-85 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med..
Tensile Strength, Yield 10.8 MPa
1560 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SPF 9020 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Good Stiffness Uses: Gaskets; Profiles; Seals Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
Tensile Strength, Yield 10.8 MPa
1570 psi
ASTM D412
Vicone High Performance Rubber VicoFluro™ 106F-BK High Performance Fluoroelastomer
Information provided by Vicone
Tensile Strength, Yield 10.8 MPa
1570 psi
Dow DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2500 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with high impact strength. It..
Tensile Strength, Yield 10.8 MPa
1570 psi
Dow Primacor® 4311 Ethylene Acrylic Acid (EAA)
PRIMACOR® 4311 polymer containing 3% comonomer 3 is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent adhesion to metallic, p..
Tensile Strength, Yield 10.8 MPa
1570 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-3985 Thermoplastic Elastomer - SBC  (discontinued **)