Polymer Property : Tensile Strength, Yield = 100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.689 MPa
100 psi
TM R050-36
Resinlab® EP1121 Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP1121 Clear is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I..
Tensile Strength, Yield 0.689 - 85.1 MPa
100 - 12300 psi
Average value: 22.8 MPa Grade Count:28
Overview of materials for Epoxy Encapsulant, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o..
Tensile Strength, Yield 0.689 MPa
100 psi
UR324; ASTM D638
Lord Adhesives Thermosetâ„¢ UR312 / UR324 Urethane Encapsulating Gel
UR312 A/B and UR324 A/B are the same components used at different mix ratios, therefore, giving different properties.LORD UR312 and UR324 are two-component, room temperature curing urethane gels. Th..
Tensile Strength, Yield 0.689 MPa
100 psi
ASTM D638
Lord Adhesives Thermosetâ„¢ UR-322 Two Component Urethane Potting Compound
Lord UR-322 is a two component, room temperature curing urethane potting compound. The cured elastomer is soft, flexible and has a very low modulus at temperatures down to -80°C. Cured UR-322 als..
Tensile Strength, Yield 0.689 MPa

@Strain 300 %
100 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP 1870 Thermoplastic Elastomer
Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on poly..
Tensile Strength, Yield 0.689 MPa
100 psi
at 100% elongation, maximum
Dow Corning SILASTIC® 25784-V SILICONE RUBBER RED
40 Durometer, peroxide cured, high temperature resistance Silicone Rubber CompoundInformation provided by Dow Corning
Tensile Strength, Yield 0.689 MPa
100 psi
ASTM D412
ACC Magnifoam™ MFSILTEC™-HD MTI Silicones Silicone Foam
Part of the Amber Chemical Group. Data provided by manufacturer.
Tensile Strength, Yield 0.689 MPa
100 psi
ASTM D412
Teknor Apex MONPRENE® MP 2137 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 0.689 MPa
100 psi
100% Secant; ASTM D638
Multibase Multi-Flex® A 2504LC TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodFoamableHardness, LowHeat StabilizedOzone ResistantProcessability, Good..
Tensile Strength, Yield 0.689 MPa
100 psi
at 100%; ASTM D412
Multibase Multi-Flex® A 2504LC TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodFoamableHardness, LowHeat StabilizedOzone ResistantProcessability, Good..
Tensile Strength, Yield 0.689 MPa
100 psi
at 100%; ASTM D412
R70-057 Styrene-based Biomedical Elastomer
Tensile Strength, Yield 0.689 MPa
100 psi
ASTM D3574
Saint-Gobain Korel® K30-20 Soft Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc..
Tensile Strength, Yield 0.689 MPa
100 psi
ASTM D3574
Saint-Gobain Korel® K30-25 Soft Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc..
Tensile Strength, Yield 0.689 MPa
100 psi
TM R050-36
Resinlab® EP1121 Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP1121 Black is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I..