Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 827 - 1069 MPa | 120000 - 155000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 MH4, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |