Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 860 - 1070 MPa | 125000 - 155000 psi | |
Materion Beryllium Copper Alloy 165 Forgings & Extrusions; AT (TF00) Temper (UNS C17000) Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 890 - 1070 MPa | 129000 - 155000 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17000) Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 860 - 1070 MPa | 125000 - 155000 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; over 51 to 76 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 860 - 1070 MPa | 125000 - 155000 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17000) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Tensile Strength, Yield | 860 - 1070 MPa | 125000 - 155000 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17000) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Tensile Strength, Yield | 930 - 1070 MPa | 135000 - 155000 psi | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM06 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation after 1000 hrs @ 200°C: 78%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Yield | 827 - 1069 MPa | 120000 - 155000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 MH4, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Tensile Strength, Yield | 931 - 1070 MPa @Strain 0.200 %, Thickness <=25.4 mm |
135000 - 155000 psi @Strain 0.200 %, Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect.. |