Mechanical Properties Metric English Comments
Tensile Strength, Yield 550 - 760 MPa
79800 - 110000 psi
Materion Beryllium Copper Alloy 10 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material..
Tensile Strength, Yield 550 - 760 MPa
79800 - 110000 psi
Materion Beryllium Copper Alloy 190 Strip; 1/4HM (TM01) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R..
Tensile Strength, Yield 676 - 758 MPa
98000 - 110000 psi
0.2% offset
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Spring
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Tensile Strength, Yield 650 - 760 MPa

@Strain 0.200 %
94300 - 110000 psi

@Strain 0.200 %
CLAL-MSX DECLAFOR® 1015 TH1 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Tensile Strength, Yield 620 - 758 MPa

@Strain 0.200 %
89900 - 110000 psi

@Strain 0.200 %
Ametek AM 388™ Alloy (UNS C72650) TM02
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Tensile Strength, Yield 550 - 760 MPa
79800 - 110000 psi
Materion Beryllium Copper Alloy 3 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17510)
Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials ..