Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 676 MPa @Temperature 23.9 °C |
98000 psi @Temperature 75.0 °F |
0° Direction, Dry; Oven Cure 250°F, 90 min; ASTM D638 |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |
|||
Tensile Strength, Yield | 676 MPa @Temperature 21.1 °C |
98000 psi @Temperature 70.0 °F |
0° Direction, Dry; Autoclave Cured; ASTM D3039-95 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 34-700 12K 2x2 Twill Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Tensile Strength, Yield | 676 MPa | 98000 psi | |
Meehanite K-295 Austempered Ductile Iron Type K-295 is used for applications such as gears requiring high contact rolling and tooth bending fatigue properties. Type K-295 also possess high fracture toughness impact strength. Excellent fo.. |
|||
Tensile Strength, Yield | 676 - 758 MPa | 98000 - 110000 psi | 0.2% offset |
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Spring Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Strength, Yield | 676 MPa @Strain 0.200 % |
98000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 593°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |