Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1140 - 1240 MPa @Strain 0.200 % |
165000 - 180000 psi @Strain 0.200 % |
|
Materion BrushCAST® 275CT Fine Grain Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Yield | 1140 - 1240 MPa @Strain 0.200 % |
165000 - 180000 psi @Strain 0.200 % |
|
Materion BrushCAST® 275C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Yield | 1140 MPa @Strain 0.200 % |
165000 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals INCOLOY® Alloy 909 A nickel-iron-cobalt alloy with a silicon addition and containing niobium and titanium for precipitation hardening. It is similar to INCOLOY alloys 903 and 907 in that it has low thermal expansion .. |
|||
Tensile Strength, Yield | 1140 MPa @Strain 0.200 % |
165000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 50% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Tensile Strength, Yield | 1140 MPa | 165000 psi | Oil Quenched from 871°C; 649°C Temper Temperature |
Latrobe Staminal™ Shock Resisting Die Steel Staminal is an air or oil hardening die steel containing a large percentage of nickel combined with a proper balance of other alloying elements for deep hardening and extreme toughness. For tools, .. |