Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 165000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1140 - 1240 MPa

@Strain 0.200 %
165000 - 180000 psi

@Strain 0.200 %
Materion BrushCAST® 275CT Fine Grain Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Tensile Strength, Yield 1140 - 1240 MPa

@Strain 0.200 %
165000 - 180000 psi

@Strain 0.200 %
Materion BrushCAST® 275C High Strength Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Tensile Strength, Yield 1140 MPa

@Strain 0.200 %
165000 psi

@Strain 0.200 %
Precipitation Hardened. Value at room temperature
Special Metals INCOLOY® Alloy 909
A nickel-iron-cobalt alloy with a silicon addition and containing niobium and titanium for precipitation hardening. It is similar to INCOLOY alloys 903 and 907 in that it has low thermal expansion ..
Tensile Strength, Yield 1140 MPa

@Strain 0.200 %
165000 psi

@Strain 0.200 %
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 50% Cold Work
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..
Tensile Strength, Yield 1140 MPa
165000 psi
Oil Quenched from 871°C; 649°C Temper Temperature
Latrobe Staminal™ Shock Resisting Die Steel
Staminal is an air or oil hardening die steel containing a large percentage of nickel combined with a proper balance of other alloying elements for deep hardening and extreme toughness. For tools, ..
Copyright © lookpolymers.com All Rights Reserved