Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 7.93 MPa | 1150 psi | ASTM D412 |
Polymax® Maxelast® P1785 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 7.93 MPa @Temperature 23.0 °C |
1150 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7680-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Tensile Strength, Yield | 7.90 MPa | 1150 psi | M100 |
3M Dyneon™ Fluorel™ FE-5660Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Tensile Strength, Yield | 7.93 MPa | 1150 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 505 Perfluoroelastomer Chemraz® 505, a perfluoroelastomer, provides a broader range of chemical resistance than any other compound on the market. With a temperature range of -22°F to 446°F (-30°C to 230°C).. |
|||
Tensile Strength, Yield | 7.93 MPa | 1150 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 565 Perfluoroelastomer Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r.. |
|||
Tensile Strength, Yield | 7.93 MPa | 1150 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 550 Perfluoroelastomer Chemraz ® 550 is recommended for use in wet systems where chemical compatibility is required and small amounts of contamination are acceptable. This seal material has a wide variety of uses in d.. |
|||
Tensile Strength, Yield | 7.93 MPa | 1150 psi | Tensile strength decreases by 15% after dry heat aging for 70 hrs at 437°F.; ASTM D412 |
Saint-Gobain COHRlastic® 9235 High Performance Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tensile Strength, Yield | 7.93 MPa | 1150 psi | ASTM D412 |
Teknor Apex APEX® 3311-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 7.93 MPa | 1150 psi | ASTM D412 |
Teknor Apex APEX® 94-A0098C-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-ClearForms-PelletsProcessing Method-Injection Molding.. |
|||
Tensile Strength, Yield | 7.93 MPa | 1150 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8068BL Thermoplastic Elastomer Elastocon® 8068BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068BL is well sui.. |
|||
Tensile Strength, Yield | 7.90 MPa | 1150 psi | |
Dow Primacor® 3340 Ethylene Acrylic Acid (EAA) PRIMACOR® 3340 polymer containing 6.5% comonomer is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent adhesion and outstandin.. |
|||
Tensile Strength, Yield | 7.90 MPa | 1150 psi | |
Dow Primacor® 3440 Ethylene Acrylic Acid (EAA) PRIMACOR® 3440 polymer containing 9.5% comonomer is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent hot tack and adhesion t.. |
|||
Tensile Strength, Yield | 7.93 MPa | 1150 psi | ASTM D-638 |
Axiall 6702 Moldings & Extrusions Flexible PVC An expandable, low gravity, injection molding compound specifically developed for footwear applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 7.93 MPa | 1150 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-4070 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionIndustrialConsumer GoodsProcessing Method:ExtrusionInforma.. |
|||
Tensile Strength, Yield | 7.93 MPa @Strain 300 % |
1150 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-5190 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalIgnition ResistantApplications:Multi-PurposeMarket:Building and ConstructionConsumer GoodsIndustrialProcessing Method:Injection Mo.. |