Polymer Property : Tensile Strength, Yield = 7.93 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.93 MPa
1150 psi
ASTM D412
Polymax® Maxelast® P1785 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 7.93 MPa

@Temperature 23.0 °C
1150 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7680-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7680-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Tensile Strength, Yield 7.93 MPa
1150 psi
@100% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 505 Perfluoroelastomer
Chemraz® 505, a perfluoroelastomer, provides a broader range of chemical resistance than any other compound on the market. With a temperature range of -22°F to 446°F (-30°C to 230°C)..
Tensile Strength, Yield 7.93 MPa
1150 psi
@100% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 565 Perfluoroelastomer
Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r..
Tensile Strength, Yield 7.93 MPa
1150 psi
@100% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 550 Perfluoroelastomer
Chemraz ® 550 is recommended for use in wet systems where chemical compatibility is required and small amounts of contamination are acceptable. This seal material has a wide variety of uses in d..
Tensile Strength, Yield 7.93 MPa
1150 psi
Tensile strength decreases by 15% after dry heat aging for 70 hrs at 437°F.; ASTM D412
Saint-Gobain COHRlastic® 9235 High Performance Silicone Solid Rubber
Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome..
Tensile Strength, Yield 7.93 MPa
1150 psi
ASTM D412
Teknor Apex APEX® 3311-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
Tensile Strength, Yield 7.93 MPa
1150 psi
ASTM D412
Teknor Apex APEX® 94-A0098C-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-ClearForms-PelletsProcessing Method-Injection Molding..
Tensile Strength, Yield 7.93 MPa
1150 psi
ASTM D412
Elastocon TPE Technologies Elastocon® 8068BL Thermoplastic Elastomer
Elastocon® 8068BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068BL is well sui..
Tensile Strength, Yield 7.93 MPa
1150 psi
ASTM D-638
Axiall 6702 Moldings & Extrusions Flexible PVC
An expandable, low gravity, injection molding compound specifically developed for footwear applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 7.93 MPa
1150 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-4070 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionIndustrialConsumer GoodsProcessing Method:ExtrusionInforma..
Tensile Strength, Yield 7.93 MPa

@Strain 300 %
1150 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® RT-5190 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalIgnition ResistantApplications:Multi-PurposeMarket:Building and ConstructionConsumer GoodsIndustrialProcessing Method:Injection Mo..