Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1220 - 1280 MPa | 177000 - 186000 psi | |
Plansee DENAL® 917 108 XXX (1) Tungsten-Nickel-Iron-Cobalt Alloy Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee. |
|||
Tensile Strength, Yield | 990 - 1280 MPa | 144000 - 186000 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17000) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Yield | 990 - 1280 MPa | 144000 - 186000 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; HT (TH04) Temper; up to 9.5 mm (UNS C17000) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Yield | 1030 - 1280 MPa | 149000 - 186000 psi | |
Materion Beryllium Copper Alloy 25 Strip; 1/4HT (TH01) Temper (UNS C17200) Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6.. |