Mechanical Properties Metric English Comments
Tensile Strength, Yield 1030 - 1250 MPa
149000 - 181000 psi
Materion Beryllium Copper Alloy 190 Strip; XHMS (TM08) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, R..
Tensile Strength, Yield 1030 - 1380 MPa
149000 - 200000 psi
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 25 to 51 mm Thickness (UNS C17200)
Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Yield 1030 - 1280 MPa
149000 - 186000 psi
Materion Beryllium Copper Alloy 25 Strip; 1/4HT (TH01) Temper (UNS C17200)
Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6..
Tensile Strength, Yield 1030 MPa
149000 psi
SSAB Tunnplat Domex® 034 BOR Oil quenched Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex® high strength steels offers a number of ..
Tensile Strength, Yield 1030 MPa
149000 psi
SSAB Tunnplat Domex® 044 BOR Oil quenched Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron ..
Tensile Strength, Yield 1030 MPa
149000 psi
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
Tensile Strength, Yield 1030 MPa
149000 psi
Bar, Rod & Forgings
CMW® 73 Copper Alloy
CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w..
Tensile Strength, Yield 1027 MPa
149000 psi
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 60% Cold Rolled (UNS S30403)
This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to ..
Tensile Strength, Yield 1027 MPa
149000 psi
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 60% Cold Rolled (UNS S30400)
This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to ..