Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 94.975 MPa @Temperature 22.8 °C |
13775 psi @Temperature 73.0 °F |
ASTM D638 |
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK) TECAPEEK™ high performance polymer has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's exceptional combination of properties al.. |
|||
Tensile Strength, Yield | 94.975 MPa @Temperature 22.8 °C |
13775 psi @Temperature 73.0 °F |
ASTM D638 |
Ensinger Tecapeek® MT Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |