Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 140 MPa | 20300 psi | ASTM D638 |
Gharda Chemicals GATONE™ 5630FC Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Tensile Strength, Yield | 140 MPa @Temperature 22.8 °C |
20300 psi @Temperature 73.0 °F |
ASTM D638 |
Ensinger Sintimid™ V-HP high-purity Polyimide (PI)
(discontinued **) SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | ISO 527 |
Grupo Repol Dinalon® A1S25 G25PV0 25% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 66 Mechanical properties are for dry as molded samples.Information provided by Grupo Repol. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2210F PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2210K PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East) VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 830F PBT+PET (Europe-Africa-Middle East) PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Tensile Strength, Yield | 140 MPa @Strain 0.200 %, Temperature 550 °C |
20300 psi @Strain 0.200 %, Temperature 1020 °F |
Annealed prior to test |
Special Metals BRIGHTRAY® Alloy 35 Electrical Resistance Alloy A nickel-iron-chromium electrical-resistance alloy for use at operating temperatures up to 1920°F (1050°C). It is similar to BRIGHTRAY alloy F but with rare-earth additions for greater resist.. |
|||
Tensile Strength, Yield | 140 MPa @Strain 0.200 %, Temperature 300 °C |
20300 psi @Strain 0.200 %, Temperature 572 °F |
Annealed prior to test |
Special Metals NILO® Alloy K Controlled-Expansion Alloy Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, mat.. |
|||
Tensile Strength, Yield | >= 140 MPa @Strain 0.200 % |
>= 20300 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 4D Deep-drawing Steel Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NH-3402F PC, 40% Glass Filled FR PC/GF material with 40% GF reinforcement that can be used in printer LSUInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East) VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East) VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | ASTM D638 |
Techmer ES Plastiblend® PA6 GF20 RM-B L NAT Nylon 6 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Low Moisture Absorption and LubricatedAppearance: BlackTPCI.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | ASTM-D638 |
Polyram Polytron P60B04 Homopolymer Polypropylene, Chemically Coupled 60% Long Glass Fiber A CHEMICALLY COUPLED PP 60% LONG GLASS FIBER WITH EXTRA LOAD OF ADDITIVES FOR DILUTION.Information provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | ISO 527 |
Polyram PlusTek RA300G7 Nylon 6.6 for Injection Molding, 35% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 35% glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | ISO 527 |
Polyram PlusTek RA301G5 Nylon 6.6 for Injection Molding, 25% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 25% glass fibers reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | ISO 527 |
Chevron Phillips Xtel® XE5030BL Polyphenylene Sulfide Alloy Xtel® XE5030BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide high ductility and impact strength along with good thermal stability.Information provided by Chevr.. |
|||
Tensile Strength, Yield | 140 - 170 MPa @Strain 0.200 % |
20300 - 24700 psi @Strain 0.200 % |
|
CLAL-MSX SICLANIC S® TB Quenched Copper Alloy SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Conditioned) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Tensile Strength, Yield | 140 - 240 MPa | 20300 - 34800 psi | |
ArcelorMittal 02 High formability steel for drawing, Cold rolled Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the automotive industry, both for visible and stru.. |
|||
Tensile Strength, Yield | 140 - 280 MPa | 20300 - 40600 psi | |
ArcelorMittal 51 High formability steel for drawing, Cold rolled Available in the following: Extragal®/Galvannealed (DX51D +Z/+ZF)Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used.. |
|||
Tensile Strength, Yield | 140 - 180 MPa | 20300 - 26100 psi | |
ArcelorMittal 05 High formability steel for drawing, Cold rolled Available in the following: uncoated (DC05) and electroglavanized (DC05+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product.. |
|||
Tensile Strength, Yield | 140 - 240 MPa | 20300 - 34800 psi | |
ArcelorMittal 52 High formability steel for drawing, Cold rolled Available in the following: Extragal®/Galvannealed (DX52D +Z/+ZF)Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used.. |
|||
Tensile Strength, Yield | 140 - 240 MPa | 20300 - 34800 psi | |
ArcelorMittal 55+AS Aluminized steel Use: Very difficult drawing, 600°< T < 800°CInformation provided by ArcelorMittal |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® ES-30GF/000 PES (Polyethersulfone), 30% Glass Reinforced, Hi-Temp
(discontinued **) Information provided by PolyOne™ Corporation |
|||
Tensile Strength, Yield | >= 140 MPa | >= 20300 psi | ASTM-D638 |
Polyram PlusTek RA320G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant 30% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | >= 140 MPa | >= 20300 psi | ASTM-D638 |
Polyram PlusTek RA321G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant 30% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON QEP35M PA6.10 LNP STAT-KON QEP35M is a compound based on Nylon 6/10 resin containing 25% Milled Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Electrically Conductive, Wear Resistant. |