Tensile Strength, Yield 100 - 140 MPa
14500 - 20300 psi
ArcelorMittal 07 High formability steel for drawing, Cold rolled
Available in the following: uncoated (DC07) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the au..