Polymer Property : Tensile Strength, Yield = 1408.1 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.7083 MPa
1408.1 psi
3.5% change after 168 hours @ 70°C; ASTM D412
Precision Polymer Engineering C70R Chloroprene Rubber
Red Iron Oxide filled, Chloroprene Rubber, 66-75 °IRHD. Flame retarding.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils. ..