Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering C70R Chloroprene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Chlorosulfonated Polyethylene Rubber
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering C70R Chloroprene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Red Iron Oxide filled, Chloroprene Rubber, 66-75 °IRHD. Flame retarding.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils. Formulated to exhibit flame retarding properties.
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
°IRHD; ASTM D1415
74
74
°IRHD, +6 change after 168 hours @ 70°C; ASTM D1415
Tensile Strength, Yield 9.38 MPa
1360 psi
ASTM D412
9.7083 MPa
1408.1 psi
3.5% change after 168 hours @ 70°C; ASTM D412
Elongation at Break 346.21 %
346.21 %
-11% change after 168 hours @ 70°C; ASTM D412
389 %
389 %
ASTM D412
Compression Set 43 %
43 %
24 hours @ 70°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 260 °C
>= 500 °F