Polymer Property : Tensile Strength, Yield = 1411 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.729 MPa
1411 psi
ASTM D412
Elastocon TPE Technologies Elastocon® 8078N Thermoplastic Elastomer
Elastocon® 8078N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078N is FDA compliant and well suited..