Material Notes:
Elastocon® 8078N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078N is FDA compliant and well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon® 8078N can be overmolded to polypropylene.Information provided by Elastocon® TPE Technologies
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength, Yield 9.729 MPa
1411 psi
ASTM D412
Elongation at Break 585 %
585 %
ASTM D412
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D412
Compression Set 24 %

@Time 79200 sec
24 %

@Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Feed Temperature 79.0 °C
174 °F
Rear Barrel Temperature 177 - 193 °C
350 - 380 °F
Front Barrel Temperature 182 - 199 °C
360 - 390 °F
Nozzle Temperature 188 - 204 °C
370 - 400 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F
Back Pressure 0.345 - 0.689 MPa
50.0 - 100 psi
Descriptive Properties Value Comments
Injection Rate Fast