Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 10.96 MPa | 1590 psi | ASTM D412 |
Precision Polymer Engineering C70M Chloroprene Rubber Chloroprene Rubber, 66-75 °IRHD. Formulated to meet British Standard BS2752 grade C70.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum.. |
|||
Tensile Strength, Yield | 11.0 MPa | 1590 psi | ASTM D638 |
LyondellBasell Petrothene® NA149000 Low Density Polyethylene, Blow Molding Grade PETROTHENE NA149000 resin exhibits an excellent balance of toughness and softness, with excellent dimensional stability. Typical applications include housewares, toys, containers and novelty items. .. |
|||
Tensile Strength, Yield | 11.0 MPa | 1590 psi | ASTM D638 |
LyondellBasell Petrothene® NA149000 Low Density Polyethylene, Sheet Extrusion Grade PETROTHENE NA149000 resin exhibits an excellent balance of toughness and softness, with excellent dimensional stability. Typical applications include housewares, toys, containers and novelty items. .. |