Polymer Property : Tensile Strength, Yield = 160100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1104 MPa

@Strain 0.200 %
160100 psi

@Strain 0.200 %
ATI Allvac® 6-2-4-6 Titanium Alloy, Heat Treatment: 885°C (1625°F) + Age
Data provided by Allvac.Applications: Intermediate-temperature jet engine applications. Blades, discs, spacers, seals. Standard, rotor/premium grades.
Tensile Strength, Yield 1104 MPa

@Strain 0.200 %
160100 psi

@Strain 0.200 %
ATI Allvac® 718 Nickel Superalloy, Heat Treatment: 982°C (1800°F) + Age
Data provided by Allvac.Applications: Jet engine rings, discs, shafts, compressor blades, seals, spacers. Fasteners, nuclear, oil & gas components.
Tensile Strength, Yield 1104 MPa

@Strain 0.200 %
160100 psi

@Strain 0.200 %
ATI Allvac® 718-OP® UNS N07718 Nickel Superalloy
Uses: Turbines and engines, fasteners, sub-surface safety valves, hot extrusion tooling, nuclear reactors.Property values are for samples in the metallurgical condition: 1800°F age.Information prov..
Tensile Strength, Yield 1104 MPa

@Strain 0.200 %
160100 psi

@Strain 0.200 %
ATI Allvac® 720 Nickel Superalloy, Heat Treatment: 1093°C (2000°F) + Age
Data provided by Allvac.Applications: Wheels, jet engine turbine discs and blades.
Tensile Strength, Yield 1104 MPa

@Strain 0.200 %
160100 psi

@Strain 0.200 %
ATI Allvac® 38-644 UNS R58640 Titanium Alloy
High-strength, metastable beta alloy. Uses: Spring wire, fasteners, torsion bars for aerospace and automotive applications.Property values are for samples in the metallurgical condition: 1600°F ann..