Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ATI Allvac® 720 Nickel Superalloy, Heat Treatment: 1093°C (2000°F) + Age

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer ATI Allvac
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® 720 Nickel Superalloy, Heat Treatment: 1093°C (2000°F) + Age.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: Wheels, jet engine turbine discs and blades.
Physical Properties Metric English Comments
Density 8.08 g/cc
0.292 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 400
400
Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 437
437
Estimated from Rockwell C value.
Hardness, Rockwell C 43
43
Hardness, Vickers 418
418
Estimated from Rockwell C value.
Tensile Strength, Ultimate 1517 MPa
220000 psi
Tensile Strength, Yield 1104 MPa

@Strain 0.200 %
160100 psi

@Strain 0.200 %
Elongation at Break 15 %
15 %
Reduction of Area 15 %
15 %
Component Elements Properties Metric English Comments
Aluminum, Al 2.5 %
2.5 %
Boron, B 0.020 %
0.020 %
Carbon, C 0.015 %
0.015 %
Chromium, Cr 18 %
18 %
Cobalt, Co 14.75 %
14.75 %
Molybdenum, Mo 3.0 %
3.0 %
Nickel, Ni 55 %
55 %
as balance
Titanium, Ti 5.0 %
5.0 %
Tungsten, W 1.25 %
1.25 %
Zirconium, Zr 0.040 %
0.040 %
Users viewing this material also viewed the following: