Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 163 MPa | 23600 psi | ASTM D638 |
Solvay Specialty Polymers Kadel® E-1130 Polyketone
(discontinued **) High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, plus superior chemical r.. |
|||
Tensile Strength, Yield | 163 MPa | 23600 psi | Type I, 5 mm/min; ASTM D638 |
LNP ULTEM® EXCP0096 Polyetherimide, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant
(discontinued **) Features: Lubricated, Electrically Conductive, Good Wear Resistance, High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This dat.. |
|||
Tensile Strength, Yield | 163 MPa | 23600 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RX06480 PA 66 LNP LUBRICOMP* RX06480 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% Lubricants. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 163 MPa | 23600 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 GF30 TL5 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Frict.. |
|||
Tensile Strength, Yield | 163 MPa | 23600 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp RF006PS PA 66 LNP* Thermocomp* RF-1006 EP HS is based on Nylon 6/6 containing Glass Fiber. Characteristics of this grade include Exceptional Processing and Heat Stabilizer.This data was supplied by SABIC-IP for .. |
|||
Tensile Strength, Yield | 163 MPa | 23600 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON OE004AE PPS - Branched LNP STAT-KON* OE004AE is a compound based on PPS - Branched resin containing 20% Carbon Fiber. Added features of this material are: Easy Molding, Electrically Conductive. |
|||
Tensile Strength, Yield | 163 MPa | 23600 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Verton RV006ESV_GY7E071 PA 66 Preliminary Data for 30% long glass fiber, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region. |