Tensile Strength, Yield 11.5 MPa
1670 psi
15% change after 70 hours @ 125°C; ASTM D412
Precision Polymer Engineering E50Q Ethylene Propylene Rubber
Peroxide cured, Ethylene Propylene Terpolymer, 46-55 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Complies with FDA code of Federal regulations title CFR21 section 177.2600. Water ..
Tensile Strength, Yield 11.5 MPa
1670 psi
ASTM D412
Precision Polymer Engineering E80E Ethylene Propylene Rubber
General Purpose, Ethylene Propylene Terpolymer (EPT) 75-85 IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet Aerospace specification DTD 5597A Grade 80. ASTM & ISO designation = E..
Tensile Strength, Yield 11.5 MPa
1670 psi
ASTM D412
Precision Polymer Engineering E80H Ethylene Propylene Rubber
Sulphur cured, white Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Feder..
Tensile Strength, Yield 11.5 MPa
1670 psi
ASTM D638
Reliance Industries Reclair M26500 Polyethylene
High flow Linear Low Density Polyethylene grade. Reclair M26500 is a butene comonomer with optimum levels of antioxidants.Characteristics:narrow molecular weight distribution, excellent processabi..
Tensile Strength, Yield 11.5 MPa
1670 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern Perflas® 9294 Perfluorinated Rubber
Perfluoro rubber for aggressive chemical service. Perflas ® 9294 seals are made of a chemical resistant perfluorinated fluoroelastomer (FFKM). Perflas 9294 seals offer outstanding resistance to..
Tensile Strength, Yield 11.5 MPa
1670 psi
ISO 527-2
Carmel Olefins IPETHENE® 830 Low Density Polyethylene
IPETHENE® 830 is a low density polyethylene injection molding grade. It exhibits high melt flow rate and high stiffness. APPLICATIONS IPETHENE® 830 is used to produce lids, containers, toys, and..
Tensile Strength, Yield 11.5 MPa
1670 psi
Radici Radilene® R 30 IE 0 3036 B Low Density Polyethylene
Shore hardness: 55 D (3s)Processable, recyclable, no charge and completely non-toxicApplication examples: coating of corrugated and non-corrugated pipe (conduit, plumbing pipe, steel pipe coating a..
Tensile Strength, Yield 11.5 MPa
1670 psi
ASTM D638
ExxonMobil Santoprene® 223-50 Thermoplastic Elastomer  (discontinued **)