Material Notes:
General Purpose, Ethylene Propylene Terpolymer (EPT) 75-85 IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet Aerospace specification DTD 5597A Grade 80. ASTM & ISO designation = EPDM.Applications: For sealing applications where good fluid resistance and low compression set are of prime importance. For continuous and/or intermittent use in contact with phosphate ester or silicone hydraulic fluids within the temperature ranges as quoted. Suitable for applications in contact with air, this material has excellent resistance to ozone. Unsuitable for use in contact with fuels, mineral oil based and diester oils and silicate fluids or greases derived from these.
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
°IRHD; ASTM D1415
90
90
°IRHD, +10 change after 168 hours @ 125°C; ASTM D1415
Tensile Strength, Yield 9.775 MPa
1418 psi
-15% change after 168 hours @ 125°C; ASTM D412
11.5 MPa
1670 psi
ASTM D412
Elongation at Break 136 %
136 %
-20% change after 168 hours @ 125°C; ASTM D412
170 %
170 %
ASTM D412
Compression Set 20 %
20 %
24 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
-40.0 °C
-40.0 °F
Temperature at which rigidity modulus shall not exceed 70 Mpa
Flash Point >= 200 °C
>= 392 °F