Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 11.6 MPa | 1680 psi | ASTM D412 |
Teknor Apex APEX® 3311-65 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 11.6 MPa | 1680 psi | ASTM D638 |
ExxonMobil LD 419.MV Wire & Cable Resin
(discontinued **) LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.Information provided by ExxonMobil Chemical |