Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 15.0 - 18.0 MPa | 2180 - 2610 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer
(discontinued **) Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P.. |
|||
Tensile Strength, Yield | 15.0 - 18.0 MPa @Thickness 2.00 mm |
2180 - 2610 psi @Thickness 0.0787 in |
50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF) Solef® 21510 PVDF copolymer has medium viscosity and is suitable for extrusion and for solution processing in lithium batteries applications.Features: Copolymer; Good Flexibility; Medium Viscosit.. |
|||
Tensile Strength, Yield | 15.0 - 18.0 MPa @Thickness 2.00 mm, Temperature 23.0 °C |
2180 - 2610 psi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers. |
|||
Tensile Strength, Yield | 15.0 - 18.0 MPa | 2180 - 2610 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer
(discontinued **) Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |