Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 15.0 - 20.0 MPa | 2180 - 2900 psi | 50 mm/min; ISO/R 527 |
Okulen® 1000 - REG PE Colored OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Tensile Strength, Yield | 15.0 - 20.0 MPa | 2180 - 2900 psi | 50 mm/min; ISO/R 527 |
Okulen® 500 - REG PE Colored OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ASTM D412 |
Precision Polymer Engineering V80D Fluoroelastomer Compound Fluoroelastomer Rubber, 75-84 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specifications DTD5612A and DTD5543B Grade 80.Applications: Mouldings which are requ.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 6600 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6000 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6000 has b.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Konduit MT00EL PP LNP* Konduit* MT00EL is a Polypropylene base resin with thermal fillers. Characteristics of this grade are Thermal Conductivity and it is Low Extraactible.This data was supplied by SABIC-IP for th.. |
|||
Tensile Strength, Yield | 15.0 - 38.0 MPa | 2180 - 5510 psi | Average value: 27.4 MPa Grade Count:45 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Tensile Strength, Yield | 15.0 - 33.9 MPa | 2180 - 4920 psi | Average value: 19.1 MPa Grade Count:6 |
Overview of materials for High Density Polyethylene (HDPE), Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Wood Filled". Each property range of values reported is minimum and ma.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | |
LyondellBasell Lupolen® 3220 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | |
LyondellBasell Lupolen® 3226 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ISO 527 |
MRC Polymers MAXTEL™ 600T18 TPO, 18% Talc Filled • For automotive exterior applications• Excellent process ability and dimensional stability• Can be UV Stabilized• Internal and external lubricants can be addedInformation pr.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ASTM D638 |
LyondellBasell Hifaxâ„¢ ETA-5061 Thermoplastic Olefin Resin Key Features: fractional melt flow, medium low modulus, blow molding grade thermoplastic olefin resin, flexible, good impact resistance, good processabilityApplications: automotive ductwork, convolu.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ISO 527-1, -2 |
LyondellBasell Hostacomâ„¢ CA270G Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CA270G fractional melt flow, 140 MPa flexural modulus, UV-stabilized thermoplastic elastomeric olefin (TEO) resin has an excellent combination of grain retention characte.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SIM 5029 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | |
Trelleborg R698 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | |
Trelleborg R848 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tensile Strength, Yield | 15.0 MPa @Strain 300 % |
2180 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® 3385A Polyurethane Extrusion- and injection molding gradegood wear resistanceshort cycle timeshigh melt stabilityApplicationhard - soft systemsHosesnon-reinforcedProfilesInjection molded engineering partsPreprocessing.. |
|||
Tensile Strength, Yield | 15.0 MPa @Strain 300 % |
2180 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 8785 A Polyurethane injection molding gradewith special UV stabilizersEasy releaseshort cycle timesApplicationSports shoe solesPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ISO 527-1/2 |
CTC SunPro® SP 200 TF 3033 Polypropylene Copolymer, 33% Talc Filled SunPro® SP 200 TF 3033 is a 33% talc filled polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Application: VW TL 52660 MD 03Data .. |
|||
Tensile Strength, Yield | 15.0 - 25.0 MPa | 2180 - 3630 psi | Spec; ISO 527-1/2 |
Axion Polymers Axpoly® PS01 3003 Enhanced White General Purpose Polystyrene PS01 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of resin co.. |
|||
Tensile Strength, Yield | 15.0 - 25.0 MPa | 2180 - 3630 psi | Spec; ISO 527-1/2 |
Axion Polymers Axpoly® PS01 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from refrigerators)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in a range of co.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437C10L Calcium Reinforced |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437M30L Mica Reinforced |
|||
Tensile Strength, Yield | 15.0 MPa @Strain 50.0 % |
2180 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,16-001High flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High burst pressure and impact strength.. |
|||
Tensile Strength, Yield | 15.0 MPa @Temperature 80.0 °C |
2180 psi @Temperature 176 °F |
ASTM Test |
BASF Ultramid® 8254 HS BK-102 PA6 (Dry) Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ASTM-D638 |
Braskem IJ33D LLDPE Injection Molding Polyethylene Copolymer IJ33D is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, excellent flexibi.. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ISO R 527 |
Addiplast Addilene J 470 ST14 Polypropylene Copolymer Soft touchInformation provided by Addiplast. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ASTM D638 |
NOVA Chemicals Sclair® 94D1 HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, high stretchability, excellent strength.Applications: Package nettings for produce, Christmas tree wrap and turkey overwrap.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | 2 in/min; ASTM D638 |
Solvay Engineered Polymers DEXFLEX® 880 TPO
(discontinued **) Description: DEXFLEX® 880 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact, good processabil.. |
|||
Tensile Strength, Yield | 15.0 - 39.0 MPa | 2180 - 5660 psi | Average value: 27.1 MPa Grade Count:65 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Tensile Strength, Yield | 15.0 - 46.9 MPa | 2180 - 6800 psi | Average value: 31.3 MPa Grade Count:14 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |