Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 18.4 MPa | 2670 psi | ASTM D412 |
Polymax® Maxelast® A9880 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Strength, Yield | 18.4 MPa | 2670 psi | ASTM D412 |
Polymax® Maxelast® P3895 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 18.4 MPa | 2670 psi | ASTM D412 |
Precision Polymer Engineering Kemex™ V76E Kemex™ ETP fluoroelastomer is a premium peroxide cured fluoroelastomer that exhibits improved fluid resistance over any FKM fluoroelastomer. It is designed for severe service applications, which re.. |
|||
Tensile Strength, Yield | 18.4 MPa | 2670 psi | ASTM D412 |
Precision Polymer Engineering Kemex™ V76W Kemex™ ETP fluoroelastomer is a premium peroxide cured fluoroelastomer that exhibits improved fluid resistance over any FKM fluoroelastomer. It is designed for severe service applications, which re.. |
|||
Tensile Strength, Yield | 18.4 MPa | 2670 psi | ASTM D412 |
Precision Polymer Engineering Kemex™ V96E Kemex™ ETP fluoroelastomer is a premium peroxide cured fluoroelastomer that exhibits improved fluid resistance over any FKM fluoroelastomer. It is designed for severe service applications, which re.. |
|||
Tensile Strength, Yield | 18.4 MPa | 2670 psi | ASTM D412 |
Precision Polymer Engineering V76E Fluoroelastomer Compound ETP polymer. This peroxide cured compound is based on a tetrapolymer of Ethylene, Tetrafluoroethylene (TFE) and Perfluoromethylvinylether (PMVE), and a cure site monomer – 70-80 °IRHD.Applications.. |