Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 18100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.1 - 125 MPa
9000 - 18100 psi
Average value: 99.3 MPa Grade Count:63
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Tensile Strength, Yield 26.2001 - 125 MPa

@Temperature -40.0 - 120 °C
3800.01 - 18100 psi

@Temperature -40.0 - 248 °F
Average value: 74.9 MPa Grade Count:2
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Tensile Strength, Yield 58.6 - 125 MPa
8500 - 18100 psi
Average value: 88.7 MPa Grade Count:10
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Tensile Strength, Yield 40.5 - 125 MPa
5870 - 18100 psi
Average value: 89.3 MPa Grade Count:61
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..
Copyright © lookpolymers.com All Rights Reserved