Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.5 MPa
5870 psi
ASTM D638
Multibase Multi-Pro® 3012 RC Polypropylene
Glass Fiber Reinforced, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Tensile Strength, Yield 40.5 MPa
5870 psi
Ineos ABS Lustran® LGA-SF  (discontinued **)
Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquir..
Tensile Strength, Yield 40.5 MPa
5870 psi
ASTM D-638
Axiall 7751 Rigid PVC, Extrusion
Georgia Gulf 7751 is a vertical blind profile exterior compound requiring the following properties: Impact Strength & ToughnessColorabilityDimensional StabilityUV Color StabilityEasy Processing in ..
Tensile Strength, Yield 40.5 - 125 MPa
5870 - 18100 psi
Average value: 89.3 MPa Grade Count:61
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..