Polymer Property : Tensile Strength, Yield = 1890 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.00 - 13.0 MPa
1020 - 1890 psi
±30% change after 70 hours @ 100°C; ASTM D412
Precision Polymer Engineering N80V Nitrile Rubber
Nitrile/PVC Rubber, 75-85 °IRHD. Copolymer of acrylonitrile and butadiene, blended with PVC. ASTM & ISO designation = NBR.Applications: Excellent resistance to petroleum based oils and fuels. Impr..
Tensile Strength, Yield 7.00 - 13.0 MPa
1020 - 1890 psi
±30% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering V71H Fluoroelastomer Compound
Green Fluoroelastomer Rubber, 70-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Federal Food and Drug Ad..