Tensile Strength, Yield 19.5 MPa
2830 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 70 PHR N550 (FEF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 19.5 MPa
2830 psi
50 mm/min; ISO 527-1,-2
Inno-Comp INNOPOL® CS 2-9514 10% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer
INNOPOL® CS 2-9514 is a 10% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9514 is dev..
Tensile Strength, Yield 19.5 MPa
2830 psi
ASTM D412
Teknor Apex Flexalloy® 9300-80 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R..
Tensile Strength, Yield 19.5 MPa
2830 psi
50mm/min; ISO 527-2
Borealis Daplen™ ED230HP Polypropylene TPO Compound
Daplen™ ED230HP is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac..
Tensile Strength, Yield 19.5 MPa
2830 psi
ASTM D638
Tipco Tipcolene® NPI 200 IN - 25% Talc/Mineral Reinforced Polypropylene Copolymer with Very High Flow, Stiffness & Impact Strength
20% Mineral Reinforced, Very High Stiffness & Very High Impact PP CopolymerApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries ..
Tensile Strength, Yield 19.5 MPa
2830 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 70 PHR N550 (FEF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 19.5 MPa
2830 psi
47% Ret.
UBE UBESTA® 3030U Nylon 12 (After Methanol for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Tensile Strength, Yield 19.5 MPa
2830 psi
ASTM D638
Tipco Tipcolene® TPE 1000 - Impact Modified Polypropylene Copolymer Compound with High Stiffness
High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Tensile Strength, Yield 19.5 MPa
2830 psi
ASTM D412
Teknor Apex APEX® 94-A0098A-90 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I..
Tensile Strength, Yield 19.5 MPa
2830 psi
ASTM D638
Tipco Tipcolene® MD-TPE MD TPE - Impact Modified Polypropylene Copolymer Compound for Automobile Bumpers
High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Copyright © lookpolymers.com All Rights Reserved