Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 20.3 MPa | 2940 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable 0860-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 20.3 MPa | 2940 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable WJLF112L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | ASTM D412 |
Polymax® Maxelast® D6890 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | heat aged 70 hours at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Friction Compound MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | |
Spartech 2850-90 PVC for Regulated Applications Information provided by Spartech |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | ASTM D 638 |
Styrolution PS 5400/5401 HIPS Good ESCRHigh ImpactLow gloss (matte finish)USP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | ASTM D 638 |
Styrolution PS 7120 HIPS Excellent ESCR to foodstuffs and PUR foamsGood low temperature impact strengthHigh relative stiffness/potential to down gauge sheetUL Classification 94 HBInformation provided by Styrolution |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | ASTM D638 |
Washington Penn Medium Impact Copolymer 10% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 2610A Compounding and Injection Molding Polypropylene High Impact CopolymerApplications: Automotive compounds, lawn and garden products, and appliances.Formolene 2610A is a high impact copolymer of polypropylene designed for such applications as automo.. |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Friction Compound MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | heat aged 70 hours at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | ASTM D638 |
Dow DT702 TPO Dow Fascia TPO for Painted ApplicationsInformation provided by Dow |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | ASTM D412 |
ACC EP LCP EPI Engineered Polymers Aromatic Polyurea EP LCP Aromatic Polyurea, “Powered by Reactamine® Technology” is a two component 100% solid Polyurea (silicone optional) with superior performance in industrial applications. EP LCP displays extr.. |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | ASTM D-638 |
Axiall 01590 Plenum Flexible PVC Non-lead stabilized plenum grade insulation compound for Category 3 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | ASTM D-638 |
Axiall 10790 Wire & Cable Flexible PVC 60C compound suitable for integral non-metallic conduit jacket 1" and larger per UL 1660.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | ASTM D-638 |
Axiall 35851 Moldings & Extrusions Flexible PVC 105C plug molding compound. UL recognized component for 94-5VA in all colors (3.0 mm min. thickness). UL QMFZ2 recognized component.Information provided by Georgia GulfGeorgia Gulf became Axiall C.. |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | ASTM D-638 |
Axiall 8901 Moldings & Extrusions Flexible PVC Outdoor grade extrusion compound formulated for good UV light resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | 2:1; ASTM D412 |
ACC EP JS EPI Engineered Polymers Joint Sealant EP JS Joint Sealant JS, “Powered by Reactamine® Technology” is a two component 100% solid (silicone optional) polyurea based joint sealant. EP JS is a self-leveling joint sealant designed to prot.. |
|||
Tensile Strength, Yield | 20.3 MPa | 2950 psi | ASTM D-638 |
Axiall 19481 Wire & Cable Flexible PVC 105°C, VW-1 rated non-lead stabilized insulation. Best suited for small gauge, 1/64 wall applications. UL approved for TW, THW, THHW, THHN-THWN insulation.Information provided by Georgia GulfGeor.. |