Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.1 MPa
3060 psi
ASTM D412
Precision Polymer Engineering Perlast® G80A Perfluoroelastomer
A black general purpose perfluoroelastomer compound with excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Do not use any P..
Tensile Strength, Yield 21.1 MPa

@Thickness 3.20 mm
3060 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOL HF5157Z PP+Rubber+MF, High Flow and Stiffness, High Impact
Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good PaintabilityApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provided by LG Chemical
Tensile Strength, Yield 21.1 MPa

@Temperature 23.0 °C
3060 psi

@Temperature 73.4 °F
ASTM D638
Ineos N20L-00 Polypropylene Impact Copolymer
This is a nucleated polypropylene impact copolymer formulated with a slip agent for improved mold release, and has an optimum balance of stiffness and impact resistance for injection molding applica..
Tensile Strength, Yield 21.1 MPa
3060 psi
Spartech M60095 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
Tensile Strength, Yield 21.1 MPa
3060 psi
Zylog Hipolyene® 6251 Y M4 C Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Tensile Strength, Yield 21.1 MPa
3060 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Solvay Engineered Polymers DEXFLEX® 925 TPO  (discontinued **)
Description: DEXFLEX® 925 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and e..