Material Notes:
Description: DEXFLEX® 925 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent processability. Applications: Bumper fascias, and other large components that must exhibit durable paintability or excellent weatherability Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ISO 1183
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
as molded; ISO 294
0.0080 - 0.011 cm/cm
0.0080 - 0.011 in/in
after bake; ISO 294
Melt Flow 30 g/10 min
30 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.1 MPa
3060 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 1.15 GPa
167 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 23.7 J
17.5 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 53.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
29.4 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228
Users viewing this material also viewed the following: