Polymer Property : Tensile Strength, Yield = 2230 MPa
Polymer Property :
Tensile Strength, Yield =
2230 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
2230
MPa
323000
psi
Hexcel® HexPly® EH04 Epoxy Resin System, IM4 Fiber
IM4 120 24" EH04 31%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel