Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 15.645 MPa | 2269.1 psi | 5% change after 72 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering Perlast® G80X Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require exposure.. |