Polymer Property : Tensile Strength, Yield = 229900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1585 MPa

@Strain 0.200 %
229900 psi

@Strain 0.200 %
<150 in<sup>2</sup>
Latrobe Dynaflex® VAC-ARC High Strength Alloy Steel
DYNAFLEX VAC-ARC steel is a medium alloyed, air hardening ultra high strength grade designed for structural applications requiring room temperature tensile strengths of 220,000 to 300,000 psi. Due ..