Polymer Property : Tensile Strength, Yield = 26.55 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.55 MPa
3851 psi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 70A
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
Tensile Strength, Yield 26.55 MPa
3851 psi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 70A
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..