Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 27.50 MPa | 3989 psi | heat aged 70 hours @ 100ºC |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Di-Cup 40C Peroxide, Hardness 66A Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 27.50 MPa | 3988 psi | At 50 mm/min; ISO 527-2 |
Borealis Bormed™ RG835MO Polypropylene Copolymer for Healthcare Applications Bormed RG835MO is specially modified polypropylene random copolymer with high melt flow intended for use in medical and medical related articles. RG835MO is modified with an internal lubricant for .. |
|||
Tensile Strength, Yield | 27.50 MPa | 3989 psi | heat aged 70 hours @ 100ºC |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Di-Cup 40C Peroxide, Hardness 66A Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |