Borealis Bormed™ RG835MO Polypropylene Copolymer for Healthcare Applications

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name Bormed™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Bormed™ RG835MO Polypropylene Copolymer for Healthcare Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bormed RG835MO is specially modified polypropylene random copolymer with high melt flow intended for use in medical and medical related articles. RG835MO is modified with an internal lubricant for products requiring a low surface friction.Bormed RF830MO is designed for use in devices such as syringes and needle hubs, blood and urine tubes, catheter connections, and screw caps and closures.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ISO 2039-2
Tensile Strength, Yield 27.50 MPa
3988 psi
At 50 mm/min; ISO 527-2
Elongation at Yield 12 %
12 %
At 50 mm/min; ISO 527-2
Tensile Modulus 1.20 GPa
174 ksi
At 1 mm/min; ISO 527-2
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 220 - 250 °C
428 - 482 °F
Mold Temperature 30.0 - 40.0 °C
86.0 - 104 °F