Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.8 MPa
4030 psi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 70A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tensile Strength, Yield 27.8 MPa
4030 psi
C.O.I.M. PLAXTER® P 05 Low Viscosity Polymeric Plasticizer
Description: Used in the field of adhesive tapes.Information provided by P.A.T. Products, Inc.
Tensile Strength, Yield 27.8 MPa
4030 psi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 70A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..