Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.86 MPa | 270 psi | at 200%, post cured- 2 hours at 177°C; ASTM D412 |
Multibase C6-265 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 1.86 MPa | 270 psi | at 150% Elongation, maximum |
Dow Corning SILASTIC® LS 5-8754 FLUOROSILICONE BASE 50 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |
|||
Tensile Strength, Yield | 1.86 MPa @Strain 100 % |
270 psi @Strain 100 % |
ASTM D412 |
Multibase Multi-Flex® A 6221 CUV A Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 1.86 MPa @Strain 100 % |
270 psi @Strain 100 % |
ASTM D412 |
Multibase Multi-Flex® A 6221 CUV A VY Dk Pewter TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Yield | 1.86 MPa @Strain 100 % |
270 psi @Strain 100 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® ST-6240 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Over-Molding GradeUV StabilizedApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |