Material Notes:
50 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc

@Temperature 25.0 °C
1.50 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 53
53
Tensile Strength, Ultimate 8.69 MPa
1260 psi
Tensile Strength, Yield 1.86 MPa
270 psi
at 150% Elongation, maximum
Elongation at Break 270 %
270 %
Tear Strength 37.9 kN/m
216 pli
Processing Properties Metric English Comments
Shelf Life 36.0 Month
36.0 Month
Descriptive Properties Value Comments
Color off-white