Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.00 - 18.9 MPa | 145 - 2740 psi | Average value: 9.12 MPa Grade Count:41 |
Overview of materials for Chlorosulfonated Polyethylene Rubber This property data is a summary of similar materials in the MatWeb database for the category "Chlorosulfonated Polyethylene Rubber". Each property range of values reported is minimum and maximum val.. |