Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Chlorosulfonated Polyethylene Rubber". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.07 - 1.70 g/cc
0.0387 - 0.0614 lb/in³
Average value: 1.24 g/cc Grade Count:20
pH 12.0
12.0
Average value: 12.0 Grade Count:4
Viscosity 45.0 - 260 cP
45.0 - 260 cP
Average value: 148 cP Grade Count:3
Mooney Viscosity 15.0 - 96.0
15.0 - 96.0
Average value: 49.6 Grade Count:40
Thickness 800 - 1590 microns
31.5 - 62.5 mil
Average value: 1330 microns Grade Count:3
Mechanical Properties Metric English Comments
Hardness, Shore A 38.0 - 105
38.0 - 105
Average value: 70.8 Grade Count:50
Tensile Strength, Ultimate 7.40 - 31.8 MPa
1070 - 4610 psi
Average value: 19.3 MPa Grade Count:42
Tensile Strength, Yield 1.00 - 18.9 MPa
145 - 2740 psi
Average value: 9.12 MPa Grade Count:41
Elongation at Break 50.0 - 750 %
50.0 - 750 %
Average value: 331 % Grade Count:42
500 - 650 %

@Temperature 50.0 - 50.0 °C
500 - 650 %

@Temperature 122 - 122 °F
Average value: 575 % Grade Count:2
Resilience 55.0 - 75.0
55.0 - 75.0
Average value: 63.1 Grade Count:12
Tear Strength Test 153 - 337
153 - 337
Average value: 271 Grade Count:8
Graves Tear Strength 28.0 - 220 kN/m
160 - 1260 pli
Average value: 112 kN/m Grade Count:15
Compression Set 8.00 - 50.0 %
8.00 - 50.0 %
Average value: 29.7 % Grade Count:10
9.00 - 69.0 %

@Temperature 70.0 - 100 °C
9.00 - 69.0 %

@Temperature 158 - 212 °F
Average value: 38.9 % Grade Count:22
60.0 - 60.0 %

@Temperature 125 - 125 °C
60.0 - 60.0 %

@Temperature 257 - 257 °F
Average value: 38.9 % Grade Count:1
60.0 - 60.0 %

@Time 79200 - 79200 sec
60.0 - 60.0 %

@Time 22.0 - 22.0 hour
Average value: 38.9 % Grade Count:1
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 - 204 °C
257 - 400 °F
Average value: 136 °C Grade Count:13
Minimum Service Temperature, Air -65.0 - -2.00 °C
-85.0 - 28.4 °F
Average value: -37.1 °C Grade Count:29
Brittleness Temperature -65.0 - -2.00 °C
-85.0 - 28.4 °F
Average value: -37.1 °C Grade Count:18
Clash Berg Stiffness Temperature -26.0 - 7.00 °C
-14.8 - 44.6 °F
Average value: -17.6 °C Grade Count:15
Flash Point 260 °C
500 °F
Average value: 260 °C Grade Count:10