Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 189 MPa @Strain 0.200 %, Temperature 199 °C |
>= 27400 psi @Strain 0.200 %, Temperature 390 °F |
|
H.C. Starck Ultra 76 Alloy (Ta 2.5%W) Benefits: Significantly improved corrosion resistance in HCl and H2SO4 acids.Minimized hydrogen embrittlement rates compared to standard NRC®76Up to 100 times lower in HCl acidUp to 10 times low.. |
|||
Tensile Strength, Yield | 189 MPa | 27400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant. |
|||
Tensile Strength, Yield | 189 MPa | 27400 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-kon EE008E PEI LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r.. |