Polymer Property : Tensile Strength, Yield = 276 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.90 MPa
276 psi
ISO 527
Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound
PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri..
Tensile Strength, Yield 1.90 MPa
276 psi
508 mm/min; ASTM D638
Dow Engage® 8130 Polyolefin Elastomer
Description: Engage® 8130 polyolefin elastomer is an ethyleneoctene copolymer with low density and a high melt index. This combination provides excellent toughness, flexibility, and ease in process..
Tensile Strength, Yield 1.90 MPa
276 psi
508 mm/min; ASTM D638
Dow Engage® 8150 Polyolefin Elastomer
Description: Engage® 8150 and Engage® 8157 polyolefin elastomers are ethylene-octene copolymers that have excellent flow characteristics and provide good impact properties in blends with polypropy..
Tensile Strength, Yield 1.90 MPa
276 psi
508 mm/min; ASTM D638
Dow Engage® 8157 Polyolefin Elastomer
Description: Engage® 8157 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio..